The polypropylene fiber properties on a data sheet are density, water absorption, melting point, tensile strength, modulus, alkali resistance, denier and length. Some of these numbers describe the polymer, so they barely change from one supplier to the next. The others, however, describe how the fiber was made, and those decide how it behaves in your mix. This guide therefore takes each line in turn and says what it means on site.
Two kinds of numbers on the sheet
First, split the sheet in two. Density, melting point, water absorption and alkali resistance belong to polypropylene itself. If one of them is far off, you are probably looking at a different polymer or a filled one. Our guide to virgin polypropylene fiber shows how to catch that before you buy.
Denier, length, tensile strength, modulus and surface finish, in contrast, are product values. The extrusion line sets them, so they differ between grades and between suppliers. As a result, these are the lines worth comparing when two quotes look alike. Iran's Code 120-4 also puts most of its acceptance limits on these product values.
Density: why the fiber floats
Polypropylene is lighter than water. A peer-reviewed review of polymer fibers for concrete gives its specific gravity as 0.90 to 0.95. This is also why a pinch of real polypropylene floats in a glass of water, while polyester sinks.

On site, density also turns a dose by weight into a dose by volume. For example, a micro fiber dose of 0.6 to 1.2 kg per cubic metre is only about 0.07 to 0.13% of the concrete by volume. A light fiber also gives more filaments per kilogram than a heavier one of the same size.
The same review also lists water absorption as zero. In other words, the fiber does not take up mix water. If the slump drops after fiber goes in, the cause is the fiber's surface area and its grip on the paste, not water soaked into the fiber.
Melting point: 160 to 170 °C
Polypropylene melts at 160 to 170 °C. Because that is far above the temperature of fresh concrete, the number matters for two other reasons.
First, it confirms the polymer. Code 120-4 calls for a melting check by DSC to ASTM D7138, because polyester melts at a much higher temperature. Second, it explains the fiber's role in fire. When micro fibers melt, they leave fine channels that let steam escape from the concrete. As a result, polypropylene micro fiber is one of the recognised methods to reduce the risk of explosive spalling. However, it does not prevent spalling on its own, and fire design remains the designer's job.
Tensile strength and modulus
Of all the polypropylene fiber properties, these two vary most between products, and they answer different questions. Tensile strength says how much stress a fiber takes before it breaks. Modulus, in contrast, says how much it stretches under that stress. A stiffer fiber stretches less, so it holds the two faces of a crack closer for the same load.
Published values cover a wide range. The same review gives tensile strength of 60 to 700 MPa and modulus of 1.5 to 10 GPa. It also notes that polypropylene is weaker and less stiff than steel fiber. Our own base polymer, for example, is rated at more than 550 MPa and at least 7.5 GPa. These are nominal values for the polymer, not a batch guarantee.

Above a certain strength, grip matters more than tensile numbers. The review reports that polypropylene fibers in normal-strength concrete usually pull out rather than snap. That is why macro fibers are often embossed or textured. ACI notes that the bond of a synthetic macrofiber comes mainly from friction. Code 120-4 still sets a floor for macro fiber, which is a tensile strength above 345 MPa.
Alkali resistance
The water in fresh and hardened concrete is strongly alkaline. Polypropylene stays chemically stable in that environment, so the alkaline water does not attack it. It also cannot rust. As a result, fibers left at the surface do not stain, and water in a crack cannot corrode them.
This is the property that makes polypropylene concrete fibers a fit for wet and salty exposure. It does not, however, make the concrete itself impermeable. Mix design, joints and curing still decide that.
Denier, diameter and length
Denier is the mass in grams of 9,000 metres of filament. Therefore a lower denier means a finer fiber. Code 120-4 uses it to draw the line between micro fiber, at 580 denier or less, and macro fiber, at 581 or more. ACI describes the same split by diameter: microfibers are about 0.01 to 0.3 mm across, and macrofibers 0.3 mm and up.
Fineness changes behaviour in the mix. A fine micro fiber gives a very large number of filaments per kilogram, which suits plastic shrinkage control. In contrast, a coarse macro fiber gives fewer, stiffer strands that carry load across a crack after the concrete hardens. Our macro synthetic fibers for concrete work in that second way.
Length also works with diameter. Code 120-4 covers fibers from 6 to 64 mm. It checks length on 30 fibers: the average must be within 10% of the stated length, and 95% must fall inside the declared range. The polypropylene fiber length guide explains how to choose between 6, 12 and 18 mm, or a macro length.
Polypropylene fiber properties at a glance
| Property | Typical value | What it tells you on site |
| Density | 0.90 to 0.95 | Floats in water, sets the volume per kg |
| Water absorption | Zero | Takes no mix water |
| Melting point | 160 to 170 °C | Confirms the polymer, melts in a fire |
| Tensile strength | By grade, macro above 345 MPa | Fiber must outlast its grip in a crack |
| Modulus | By grade | Stiffer fiber holds a crack tighter |
| Alkali resistance | Stable | No attack in concrete, no rust |
| Denier | Micro up to 580, macro 581 and up | Micro or macro, and how the mix feels |
| Length | 6 to 64 mm | Matches the job, checked on 30 fibers |
What to ask for with the data sheet
A data sheet lists nominal values. So before an order, ask which test method stands behind each line. ASTM D7508, the ASTM specification for polyolefin fibers in concrete, for example, names denier, finish content, tensile strength and cut length. Also ask for the batch certificate that ties the numbers to the bags you receive. Iran's rules for these checks are summarised in our note on Code 120-4.
Finally, remember what no fiber sheet shows. Polypropylene fiber properties describe the fiber, not your concrete. For a macro grade, the number a designer uses is residual strength, measured on concrete beams or panels at your dose. A good concrete fiber supplier issues the test report for the method your specification names. Polyguard makes every grade from 100% virgin polypropylene, checks each batch in its own laboratory and sends a free sample for a trial mix.
Frequently Asked Questions
What is the density of polypropylene fiber?
A peer-reviewed review gives polypropylene a specific gravity of 0.90 to 0.95, so it is lighter than water and floats. It also absorbs no water, so it does not take up mix water.
What is the melting point of polypropylene fiber, and why does it matter?
Polypropylene melts at 160 to 170 °C. A DSC melting check confirms the polymer, and in a fire the melted micro fibers leave channels for steam, which makes them one of the recognised methods to reduce explosive spalling risk.
How do I tell micro from macro fiber on a data sheet?
Look at the denier. Code 120-4 treats 580 denier or less as micro fiber and 581 or more as macro fiber. ACI describes the same split by diameter, with macrofibers 0.3 mm and thicker.
Is polypropylene fiber resistant to the alkalinity of concrete?
Yes. Polypropylene stays chemically stable in the alkaline water of concrete and cannot rust, so fibers at the surface do not stain.
What should I ask for besides the data sheet?
Ask which test method stands behind each value and for the batch certificate of the bags you receive. For a macro grade, ask for the residual strength test report at your dose, because no fiber sheet shows it.